Dunked a stubborn forge weld in a bucket of cat litter and it held
So I'd been fighting a billet of 1084 and 15n20 for two days, and every weld I tried popped apart at the edges the second I touched it with the hammer. My neighbor Ray, who's been smithing out of his garage in Akron since the 80s, watched me cuss at it for ten minutes and then told me to bury the whole thing in a bucket of oil-dry clay litter straight out of the fire and let it sit overnight. I figured he was messing with me, but I tried it, and the next morning that weld was solid as a rock, no scale, no cold shunt, nothing. Something about the slow even cool in the clay kept the flux from drying it out funny, I guess, because I've done it three more times since and it works every time. Ray just shrugged and said his old mentor did it with ash from the coal forge, so I'm curious if anyone here has a cooling trick that sounds this dumb but actually works.